The acid value represents a higher number of carboxyl groups (- COOH) on the resin, which are essentially strong hydrophilic groups. At the same time, carboxyl groups bring more ionizable sites, making them easier to absorb water, hydrolyze, and be soaked by water. The macroscopic manifestation is a decrease in water resistance. Let’s clarify the mechanism below and distinguish the easily confused points: why is sometimes high acid value used to make water dispersible resins?
Acid value AV: The mg of KOH required to neutralize 1g of resin directly reflects the content of free carboxyl groups
1. Carboxylic groups are inherently hydrophilic
Carboxyl is a polar hydrophilic group:
\(\ce{-COOH <=> -COO- + H+}\)
Carboxyl and carboxylate groups can form hydrogen bonds with water molecules to adsorb and bind water;
The higher the acid value, the higher the density of hydrophilic sites on the resin chain, making it easier for water molecules to penetrate into the interior of the paint film;
After water enters, it plasticizes the resin, causing the paint film to soften, adhesion to decrease, whitening, and bubbling.
Comparison: Pure hydrocarbon chains, ester bonds, and epoxy bonds have weak polarity and are hydrophobic; Carboxyl groups are typical hydrophilic groups.
2. Exposure to water ionization, osmotic pressure effect (common cause of paint film bubbling)
When the paint film comes into contact with water (especially water containing electrolytes), carboxyl groups dissociate into carboxylate anions:
Fixed on the resin skeleton, it adsorbs cations (such as Na+, Ca ^ {2+}) in the system to maintain electrical neutrality;
Ions accumulate inside the paint film, forming osmotic pressure, and external water is continuously drawn into the interior of the coating;
The continuous enrichment of water leads to bubbling and peeling, which is a very typical mode of failure for high acid resin coatings when soaked in water.
3. Carboxyl catalyzed hydrolysis of ester bonds (long-term water resistance, deterioration due to wet heat aging)
Many resins are polyester and acrylic esters, with ester bonds in the main chain:
Free carboxyl groups are acidic catalysts;
Penetrating water+carboxyl catalysis → accelerates ester bond hydrolysis and chain breakage;
The molecular weight of the resin decreases, cross-linking is disrupted, and the paint film quickly loses strength and powder.
Note: It is not the carboxyl group itself that breaks the chain, but it acts as an acid catalyst, amplifying hydrolysis.
4. Matching issues of solidification system
1. Amino curing (baking paint): High acid value and quick reaction with amino groups, but if there is an excess of carboxyl groups that have not fully participated in cross-linking, residual free carboxyl groups remain in the paint film, which is a permanent hydrophilic point; When the curing is insufficient, it can withstand sudden drops in water resistance.
2. Epoxy curing: Carboxyl groups react with epoxy, and if the equivalents do not match, carboxyl groups remain.
3. Self crosslinking acrylic acid: Carboxyl groups are only used for alkaline thickening/dispersion and do not participate in crosslinking. They are all retained in the dry film and have poor water resistance.
✅ Key distinction: Water dispersible resins are intentionally made with high acid values in order to neutralize with amines and form salts, thereby obtaining water dispersibility; The cost is that if salt/carboxyl residues remain in the dry film, the water resistance is greatly sacrificed. So in water-based formulas, efforts are made to neutralize and then crosslink, crosslink and block carboxyl groups after use, or use a low acid core high acid shell structure to reduce free carboxyl groups in the dry film.
5. Side effects of interface adhesion (substrate side)
Carboxyl groups have good adhesion to metal and inorganic substrates, but conversely:
In humid environments, carboxyl groups preferentially interact with water, and water replaces the hydrogen bonds between the resin substrate, resulting in “water displacement”;
The adhesion quickly decreases under humid and hot conditions, which means poor wet adhesion.
Confusing counterexample: When will high acid value resins not have significantly poor water resistance?
Only when: almost all carboxyl groups participate in the crosslinking reaction, and there are no residual free carboxyl groups/carboxylate salts in the dry film
For example, carboxyl polyester+epoxy curing, precise equivalent ratio, high temperature sufficient reaction, carboxyl consumption is clean;
At this point, high acidity only provides cross-linking sites, and the finished film has few hydrophilic groups, so the water resistance will not significantly decrease.
It is difficult to achieve 100% reaction in reality, so under the same system and curing conditions, the higher the acid value, the more residual carboxyl groups, and the poorer the water resistance are common rules.