news

Phosphate esters are mainly used for wet adhesion, salt spray resistance, and passivation of metal substrates; Titanate is a broad-spectrum coupling agent that balances filler dispersion and multiple substrates, with a low addition amount. However, it has weaker long-term wet adhesion to metals compared to phosphate esters

1、 Mechanism of action

Phosphate esters (acidic phosphate esters, epoxy phosphate esters, polyphosphate esters)

Phosphate groups (- PO (OH) ₂) and metal surface oxides/hydroxyl groups undergo acid-base coordination to form stable P-O-M (Fe-O-P, Al-O-P, Zn-O-P) bonds, while also having a slight passivation effect on the metal surface; The other end of the organic chain segment is compatible, entangled, or reacted with the resin.

Essence: Interface passivation+chemical bonding, forming a phosphate complex layer at the interface, blocking the penetration of water and salt ions

Characteristics: Acidic, self-contained proton, no need for substrate, must have a large number of hydroxyl groups

Titanium esters (monoalkoxy, pyrophosphate, chelating titanium esters)

The central Ti atom, one end alkoxy/chelating group, and active hydrogen (proton) on the surface of the substrate react to form Ti-O-M; On the other end, multiple organic functional chains (carboxyl, phosphate, alkyl, etc.) are compatible/entangled with the resin; Single point anchoring is the main method, which is not easy to form a continuous dense interface layer .

Essence: Proton reactive coupled bridge, independent of hydrolysis; Silane must be hydrolyzed, titanium esters do not need to be hydrolyzed

Characteristics: Multi functional side chains, naturally capable of dispersing pigment fillers (calcium carbonate, barium sulfate, titanium dioxide, carbon black)

Project: Phosphate ester adhesion promoter, Titanium ester coupling agent

Best substrate cold-rolled steel, galvanized sheet, aluminum, alloy (preferred for metals); Partially modified versions can be used as inorganic fillers such as PET, PVC calcium carbonate, barium sulfate, titanium dioxide, carbon black, etc; ABS、PVC、 Some plastics and metals are interchangeable, but metals generally adhere wet

Addition amount of 1.0-5.0% (total formula) 0.3-1.5%, higher efficiency

System sensitivity acidity; It is prone to flocculation with alkaline pigments, aluminum powder, and zinc powder; It will accelerate the reaction of two-component PU and amino baking system, which is prone to shrinkage and gelatinization, posing a risk of ester exchange for ester bonds and carboxyl groups; Not resistant to strong acids and alkalis; Part of the common alkoxyl type rapidly inactivates when exposed to water

Advantages of water resistance/salt spray resistance (wet adhesion), significantly improved wet adhesion and salt spray resistance, suitable for anti-corrosion, coil, and electrophoretic primer dry adhesion is still acceptable, but the interface is prone to delamination under long-term immersion and salt spray, making it unsuitable as the main adhesion agent for anti-corrosion

Dispersion does not significantly improve the dispersion of fillers. Some polyphosphates have certain wetting strengths, reducing viscosity and preventing filler agglomeration. They are classic additives for powder modification

The storage stability of water-based systems should be controlled by pH; acidity will slowly erode packaging and affect resin stability. Ordinary monoalkoxy types are prone to deactivation when exposed to water vapor; Chelated type has better hydrolysis resistance and higher price

Baking stability is stable at medium and high temperatures. Many standard baking paint schemes for coil materials are prone to yellowing and decomposition at high temperatures, and some varieties may affect the weather resistance of the paint film

The cost is moderate, and domestic mass production is generally higher than that of ordinary phosphate esters

Typical scenarios include coil primer, automotive primer, hardware anti-corrosion, galvanized parts, aluminum powder paint, water-based metal paint, plastic filling modification, color masterbatch, powder surface treatment, ink plastic substrate, non anti-corrosion single coating

3、 Key selection points

✅  Choose phosphate esters, if you:

The substrate is made of steel, galvanized sheet, and aluminum, requiring resistance to salt spray, boiling water, and wet adhesion

Make anti-corrosion primer, coil coating, hardware baking paint, and electroplating topcoat

Need to simultaneously enhance adhesion and achieve a certain level of passivation and rust prevention effect

Attention: Acidic! The alkaline system and aluminum silver paste system must undergo compatibility testing first, as they are prone to blackening and flocculation

✅  Choose titanium esters, if you:

The main purpose is to disperse fillers and reduce viscosity (barium sulfate, calcium carbonate, titanium dioxide)

The substrate is filled with PVC/ABS and other plastics, inorganic powders, and does not pursue long-term water and corrosion resistance

I want a low addition amount that balances adhesion and dispersion, and I don’t want to add two types of additives

Attention: Do not expect titanium esters to replace phosphoric esters for heavy anti-corrosion wet adhesion; PU、 Beware of ester exchange and curing abnormalities in polyester systems


Post time: Nov-18-2026