news

The acid value represents a high content of carboxyl groups (- COOH) in the resin, which are strong hydrophilic groups; The higher the acid value, the more hydrophilic sites there are, and the easier it is to be soaked and absorb water after film formation, resulting in a decrease in water resistance at the macro level.

Attention: This is a general rule, not an absolute one – if the carboxyl group is fully cross-linked and capped afterwards, high acid value resins can also be well water-resistant.

1、 Mechanism disassembly

1. Carboxylic groups are inherently hydrophilic

Carboxylic groups have strong basicity and can form hydrogen bonds with water molecules;

· Free carboxyl groups on the surface and inside of the membrane, which is equivalent to burying a large number of “water absorption channels” in the coating;

After water seeps in, it can also cause swelling, decreased adhesion, whitening, and foaming.

The ionization effect of carboxyl groups causes water to enter the coating:

\(\ ce {R-COOH<=>R-COO -+H+} \) Carboxylates \ (\ ce {R-COO -} \) have much stronger hydrophilicity than carboxyl groups, and their water absorption will be further amplified; If there are amines, bases, and metal ions (such as pigments, fillers, and additives) in the system, carboxylate salts will be generated, which have higher solubility and are resistant to sudden drops in water.

This is also the reason why many high acid acrylic acid, polyester, and alkyd acids have poorer water resistance after neutralization and amine neutralization.

2. Impact on curing crosslinking system

· ✅  Positive: Carboxyl groups are cross-linking sites (cross-linked with epoxy, aziridine, isocyanate, and metal ions), and high acid values can increase cross-linking density;

· ❌  Negative: Only the reacted carboxyl groups will be capped and lose hydrophilicity; All unreacted residual carboxyl groups are hydrophilic defects. Many formula misconceptions: high acid value resin, insufficient proportion of curing agent, inadequate curing conditions, mismatched reaction activity → large amount of COOH residue → water-resistant direct overturning.

3. High acid value resins that affect membrane density generally have high polarity and poor compatibility with non-polar components (solvents, leveling agents, defoamers, some wax powders, low polarity resins):

Easy to cause phase separation and micropores;

Water is more likely to penetrate along interfaces and micropores; The pot that appears to have an acid value is essentially a combination of pore defects caused by decreased compatibility and hydrophilic carboxyl groups.

2、 Two easily confused counterexamples

1. High acid value+sufficient crosslinking agent, carboxyl group almost completely reacts and ends, with low residual carboxyl base; At this point, high acid value is only used to provide crosslinking points, with few free hydrophilic groups and excellent water resistance (such as partially epoxy cured high acid acrylic acid and aziridine crosslinked water-based resins).

2. High acid value, but the resin main chain is a highly hydrophobic skeleton (long carbon chain, aliphatic ring, hydrogenated bisphenol, high aromatic ring), and the contribution of the hydrophobic skeleton outweighs the hydrophilic effect of a small amount of carboxyl groups.

Comparison: Low acid value resin has fewer carboxyl groups, even if the cross-linking is slightly insufficient, there are fewer residual hydrophilic groups, and the lower limit of water resistance is higher.

3、 Common adjustment directions for improving water resistance with high acid value resin

1. Calculate the cross-linking equivalent to ensure sufficient reaction of carboxyl groups; Prioritize the use of curing systems that can react with carboxyl groups (such as epoxy, aziridine, blocked isocyanates, etc.);

2. Avoid using strong bases/large amounts of amines to neutralize and minimize the formation of carboxylate salts; Priority control of neutralization degree in water-based systems;

3. Paired with hydrophobic monomer modified skeleton (styrene, long-chain alkyl acrylate, cycloaliphatic monomer) to enhance the hydrophobicity of the main chain;

4. Control alkaline impurities in pigments/fillers (calcium carbonate, some active pigments and fillers may form salts with carboxyl groups);

5. Add a small amount of hydrophobic additives, wax, and silicon additives for surface shielding (treating symptoms, cannot solve the problem of residual carboxyl groups absorbing water internally);

6. Optimization of film-forming conditions: Heating up, extending baking, promoting sufficient crosslinking of carboxyl groups, and reducing unreacted groups.

4、 Quickly distinguish between two failure modes

After soaking in water, the overall whitening, swelling, and weight gain are significant: typical free carboxyl/carboxylate salts absorb water;

After soaking in water, bubbles and delamination occur along the interface, and the coating itself does not turn white much: carboxyl groups increase the water sensitivity of the interface, and water permeates along the substrate interface.


Post time: Nov-19-2026