Water based aluminum powder paint: mechanism and scheme of hydrogen evolution inhibition+complete directional arrangement of aluminum powder

Core contradiction: Aluminum powder is a reactive metal, while water-based systems contain water pH、 Resin and additives jointly trigger the reaction between Al and water to produce hydrogen (2Al+6H ₂ O → 2Al (OH) ∝+3H ₂↑); At the same time, aluminum powder is flake like and requires stable and controllable directional arrangement to achieve high metallic feel, high coverage, and smooth mirror effect. The two often interfere with each other: improper hydrogen suppression treatment can damage the surface lubrication of aluminum powder, directly disrupting its orientation; Directional additives may also affect the stability of passivation films and exacerbate hydrogen evolution.

1、 Principle of aluminum powder hydrogen evolution (aqueous system)

1. The primary oxide film (Al ₂ O3) on the surface of aluminum powder is very thin and easily soluble under alkaline conditions (pH>8.5). Bare aluminum reacts directly with water to release hydrogen gas; Corrosion and hydrogen evolution occur under acidic conditions with pH<5. The safety window is generally pH 6.5-8.0

2. There are two types of surface treatment methods for aluminum powder:

Floating aluminum powder: coated with stearic acid, hydrophobic, suitable for solvent based; Directly entering water can easily cause delamination, rapid hydrogen evolution, aggregation, and blackening

Non floating water-based aluminum powder (pre passivated): Silane/phosphoric acid/chromate (chromium based prohibited), organic passivation coating, is the mainstream of water-based paint

3. Causes of accelerated hydrogen evolution:

System free acid/base, amine neutralizing agent (ammonia water, triethylamine are the most harmful to aluminum powder)

· Resin contains free carboxyl groups and high acid value acrylic lotion

Pigments and fillers introduce heavy metal ions (Fe ³ ⁺, Cu ² ⁺, galvanic corrosion)

High temperature storage, sealed tank, thick coating, high solid content, high water activity

2、 Hydrogen evolution suppression scheme

1. Aluminum powder substrate selection

✅  Priority selection: Silicon coated waterborne aluminum powder (silicon dioxide coated aluminum powder) SiO ₂ dense inorganic film isolates water, is resistant to hydrolysis, and balances passivation and later orientation; It is currently the mainstream water-based aluminum powder paint. Secondly, phosphate ester passivated aluminum powder (low cost, weaker water resistance than silicon coating, strict pH control) ❌  It is not recommended to directly use solvent based floating aluminum powder and water-based paint, as hydrogen suppression is extremely difficult and prone to gas expansion.

Attention: Silicon coated aluminum powder is not completely non reactive, but the reaction rate is significantly reduced, and it can only be stabilized for a long time with the help of additives.

2. pH system control

Target pH: 7.0-7.8, try not to exceed 8.2

Neutralizer: Avoid ammonia water and small molecule amines; Recommended dimethyl ethanolamine DMEA and AMP-95 (relatively mild); Try to add as little as possible to avoid free amines attacking the aluminum powder coating

· High acid value lotion shall be used as little as possible, or low acid value, post crosslinking acrylic lotion shall be used

3. Special hydrogen suppression and corrosion inhibitor (aluminum specific)

1. Organic phosphate esters (aluminum corrosion inhibitors): adsorb on the surface of aluminum, repair oxide films, and inhibit anodic corrosion; Attention: Some phosphate esters can affect the slip orientation of aluminum powder, resulting in increased fogging and decreased metallic feel

2. Silane coupling agent: KH550 should be used with caution (amino alkaline); Recommended KH560, KH570, and aluminum powder surface hydroxyl bonding to strengthen SiO ₂ coating, while assisting in resin bonding

3. Bismuth nitrate/vanadate (chromium free passivation): passivation reinforcement, suitable for high water resistance systems; The addition amount is extremely low, excessive amount will cause blackening and extinction

4. Commercial products: water-based aluminum powder stabilizer, aluminum hydrogen suppressant (used exclusively by many coating manufacturers, compound corrosion inhibitor+chelating agent)

Chelating agent: EDTA should be used with caution as it may dissolve the passivation film on the aluminum surface; Prioritize low chelating ion blocking agents to capture heavy metal ions and prevent galvanic corrosion

4. Avoiding formula and process

Aluminum powder should not be directly ground at high speed with the original solution water or neutralizing agent: aluminum powder should be pre impregnated and dispersed (alcohol ether, cosolvent+dispersant) to make aluminum powder slurry, and then slowly added to the paint base

Co solvents: propylene glycol methyl ether, dipropylene glycol methyl ether, reduce water activity and minimize contact between water and aluminum; But it cannot be excessive, as it will affect VOC and orientation

Filler: Avoid talc powder, iron red, etc. containing heavy metal impurities; Try to use high-purity fillers as much as possible

Storage: Avoid storing at temperatures above 40 ℃

3、 Directional arrangement mechanism of aluminum powder (flake aluminum powder)

Ideal state of flake like aluminum powder: stacked parallel to the surface of the paint film, with mirror reflection of light, strong metallic feel, and good coverage; Disorderly orientation, vertical orientation, stacked folds → flower formation, grain formation, uneven metal distribution, silver shimmer. The core driving forces of orientation are the leveling of the paint film drying process, the surface shrinkage caused by solvent evaporation (buoyancy effect), and the lubrication isolation of additives, two classic theories:

1. Convection orientation: During volatilization, the surface tension gradient causes aluminum powder to be carried to the surface and spread out in the surface leveling layer

2. Isolation lubrication: There is a lubricating film between the aluminum powder sheets to reduce friction, prevent adhesion, and provide opportunities for sliding and leveling

Key conflict points: The hydrogen suppression passivation film (SiO ₂/phosphate film) itself is hydrophilic. If the surface tension is too high, aluminum powder is prone to clumping and difficult to slip and orient; Directional lubricating additives (fatty acid, wax, polyolefin wax lotion) will cover the passivation film, which may damage the hydrogen suppression effect and lead to slow hydrogen evolution in the later period – this is the balance point of water-based aluminum paint that is most difficult to adjust!

4、 Selection and Usage of Directional Alignment Additives

1. Polyethylene wax lotion (PE wax) and polypropylene wax lotion are most commonly used to form a thin layer of lubrication on the surface of aluminum powder, reduce friction between sheets, and help aluminum powder slip and lay flat in the drying stage; Disadvantages: Adding too much, the water resistance of the paint film decreases, the hydrogen suppression stability deteriorates, and the interlayer adhesion decreases; The addition amount is generally 2% to 6% of the amount of aluminum powder

2. Organic silicon leveling agent (polyether modified silicon) regulates surface tension, improves surface leveling, reduces shrinkage, and assists in orientation;   ❌  High mobility silicon and pure siloxane should be used with caution, as they are prone to floating on the surface layer and aluminum powder being pressed on the lower layer, resulting in poor orientation, fogging, and affecting recoating

3. Acrylic leveling agent is silicon free, balancing leveling and orientation friendly. It has little interference with aluminum powder passivation film and is suitable for systems that require re coating

4. Dispersants are not ordinary anionic dispersants! Anionic dispersants are prone to adsorb onto aluminum powder passivation films, disrupting passivation and inducing hydrogen evolution.   ✅  Priority: Polymer non-ionic dispersants, controlled flocculation dispersants, specialized aluminum powder dispersants; Aluminum powder coating, isolation, without damaging the passivation layer.

The impact of process on orientation

1. Spraying: If the viscosity, dilution ratio, atomization pressure, and gun speed are too low, the aluminum powder will sink; The viscosity is too high, the leveling is insufficient, and there is no time to level it; Flash evaporation time: There must be appropriate flash evaporation to allow the co solvent to slowly evaporate and give the aluminum powder slip time; Flash drying too fast, aluminum powder is directly fixed in a disorderly direction; Flash drying is too slow, causing aluminum powder to sink and sag.

2. Paint film thickness: Aluminum powder orientation has an optimal film thickness range, generally 15-35 μ m; The film is too thick, causing turbulence in convection and a decrease in orientation.

3. Baking conditions: Low temperature baking (60-80 ℃) is better than high temperature rapid baking; Rapid crust formation on the surface during rapid drying, aluminum powder being locked in, and poor orientation.

5、 Core formula balance approach

1. Choose silicon coated water-based aluminum powder for aluminum powder, do not use ordinary aluminum phosphate powder to make high metal mirror silver

2. Pre dispersion of aluminum powder: aluminum powder+cosolvent+special aluminum powder dispersant+a small amount of wax lotion, which is first made into aluminum slurry, not mixed with lotion and neutralizer in advance

3. pH control 7.0-7.8, use AMP-95/DMEA, adjust a small amount multiple times, and then add aluminum paste after adjustment

4. Corrosion and hydrogen suppressants: Low addition amount (0.2-1%), priority should be given to organic phosphate aluminum specific corrosion inhibitors, and small-scale tests should be conducted to confirm that they do not damage the orientation

5. Wax lotion shall be selected with low migration and low hydrophilic brand number, and the addition amount shall be gradually increased from the lower limit to the upper limit; Priority is given to acrylic leveling with leveling agent, and a small amount of testing is required for silicon leveling

6. Conduct simultaneous testing of two indicators for small-scale evaluation:

Hydrogen evolution: Sealed and stored at 50 ℃ for 7 days, observe the swelling, pH changes, and blackening of aluminum powder inside the tank

Orientation: Spray sample, visually inspect the metal uniformity, flash, and aluminum powder layout under a microscope

6、 Corresponding investigation of common diseases

1. Tank bloating, drum bulging → hydrogen evolution: high pH, damaged aluminum powder coating, excessive free amines, heavy metal ion pollution, wrong selection of aluminum powder

2. Poor orientation, mottled, uneven brightness of aluminum powder: flash drying too fast/too slow, incorrect viscosity, insufficient wax, wrong dispersant selection, excessive silicon leveling

3. Hydrogen suppression has stabilized, but the metal sensitivity is weak and fogging occurs: the addition of phosphate esters/corrosion inhibitors forms a misty adsorption layer on the aluminum surface

4. The orientation is very good at the initial stage, and it will blossom after storage for a period of time: wax lotion and aluminum powder passivation film will slowly desorb, and aluminum powder will agglomerate