The sulfuric acid process is old, the raw materials are cheap, and it can produce rutile and rutile, but there is a lot of waste residue and acid; The chlorination method can only produce rutile with narrow particle size distribution, better whiteness and coverage, and less solid waste, but the raw materials are expensive and the technical threshold is extremely high
1、 Process route
✅ Sulfuric acid method for titanium iron ore/titanium slag+concentrated sulfuric acid hydrolysis → iron removal and purification → water splitting to produce titanium dioxide → water washing and calcination → intermittent/semi continuous process for titanium dioxide, mainstream process in China
✅ Chlorination method for high-grade rutile/synthetic rutile+coke+chlorine gas high-temperature chlorination → crude titanium tetrachloride → distillation purification → high-temperature gas-phase oxidation → titanium dioxide fully continuous gas-phase process, chlorine gas circulation
2、 Core Comparison Table
Project sulfuric acid method and chlorination method
Raw material ilmenite (low-grade, cheap), titanium slag; Raw materials are readily available in both synthetic and natural forms, with TiO ₂ ≥ 85%. However, raw materials are expensive and resources are scarce
Both anatase and rutile crystal types can be produced, and only rutile crystal types can be produced
The particle size distribution is wide and narrow, with good consistency and higher coverage
Whiteness and background color tend to be yellowish (with a higher b-value) and bluish white, resulting in a cleaner background color
Impurities are more prone to residual metal impurities such as iron and vanadium, with weak weather resistance and thorough distillation for impurity removal. The impurities are low and the weather resistance is excellent
The dispersibility is average, and it is better to have a high dependence on the coating. It is easy to disperse in coatings and plastics
A large amount of green alum and dilute waste acid are produced as environmental by-products, with high environmental pressure and less solid waste. Chlorine gas is circulated, and the pressure of the three wastes is low
Mature and low technological barriers, high barriers to entry for domestic manufacturers’ multi-core oxidation technology, and equipment that is resistant to high temperatures and corrosion
The cost of ore is cheap, but the cost of waste acid treatment is high. Ore is expensive, and equipment investment is huge
3、 Performance and Applicable Scenarios
Chlorinated gold red stone (high-end)
Advantages: Strong coverage, good whiteness, excellent weather resistance, stable color difference. Suitable for high-end exterior wall coatings, automotive paints, high-end plastics, color masterbatch, films, high-end inks, outdoor products
Attention: Trace chlorine, very few chlorine sensitive systems cannot be used
Sulfuric acid titanium dioxide
1. Sulfuric acid method anatase type (A): good extinction, acceptable whiteness, and low price; Suitable for interior wall coatings, papermaking, synthetic fiber extinction, rubber, ordinary ink, with poor weather resistance, not suitable for outdoor use
2. Sulfuric acid method gold red stone (R): cost-effective option; Suitable for ordinary industrial paint, powder coating, low-end plastic, putty, with weaker outdoor weather resistance than chlorinated gold red stone
4、 Simple purchasing suggestions
Interior wall, papermaking, extinction → sulfuric acid method for rutile
Limited budget, ordinary indoor paint, ordinary plastic → sulfuric acid method gold red stone
Exterior walls, outdoor areas, automotive paint, high demand colorants, high gloss systems → Priority chlorination method for gold red stone
Post time: Nov-20-2026